Asme SA213 , ASTM a 213 T5, T11, T12, T22, T91, seamless steel pipes for heat exchangers

C&N offers high quality of  ASME SA213, ASTM A 213 T2, T11, T12, T22, T91,  heat-Exchanger seamless steel tubeFeatures:(1) Commodity:Application: Boiler tube, super heater tube, heat-Exchanger tube.(2) Process method: Cold drawn / cold rolled(

Featured Products

C&N offers high quality of  ASME SA213, ASTM A 213 T2, T11, T12, T22, T91,  heat-Exchanger seamless steel tube

Features:
(1) Commodity:Application: Boiler tube, super heater tube, heat-Exchanger tube.
(2) Process method: Cold drawn / cold rolled
(3) Surface finish: Anneal / pickling / polished / bright anneal
(4)Material details

Standard: ASTM A213/ASME SA213
Steel grade: T2, T11, T12, T22, T91, T92
Size: OD (10-127mm) x WT (1.2-12.7mm)



Grade
Chemical Composition%
CSiMnP,SCrMoNiVAl
T20.10~0.200.10~0.300.30~0.61≤ 0.0250.50~0.810.44~0.65---
T110.05~0.150.50~1.000.30~0.60≤ 0.0251.00~1.500.44~0.65---
T120.05~0.15≤ 0.50.30~0.61≤ 0.0250.80~1.250.44~0.65---
T220.05~0.15≤ 0.50.30~0.60≤ 0.0251.90~2.600.87~1.13---
T910.07~0.140.20~0.500.30~0.60≤ 0.028.0~9.50.85~1.05≤ 0.40.18~0.25≤ 0.015
T920.07~0.13≤ 0.50.30~0.60≤ 0.028.5~9.50.30~0.60≤ 0.40.15~0.25≤ 0.015
GradeChemical Composition%Mechanical Properties
WBNbNT. SY.PElongationHardness
T2----≥415MPa≥205MPa≥30%163HBW ( 85HRB)
T11----≥415MPa≥205MPa≥30%163HBW ( 85HRB)
T12----≥415MPa≥220MPa≥30%163HBW ( 85HRB)
T22----≥415MPa≥205MPa≥30%163HBW (85HRB)
T91--0.06~0.100.03~0.07≥585MPa≥415MPa≥20%250HBW (25HRB)
T921.50~2.000.001~0.0060.04~0.090.03~0.07≥620MPa≥440MPa≥20%250HBW (25HRB)


(5) Packaging: Seaworthy wooden cases / steel framed cases / simple packaging

Contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours
li>
  • FAQ
  • About us
  • Contact us
  • Hot Tags

    Copyright © 2021 Dongguan jiabo Pipe Co., Ltd. Sitemap